1. Put the pure water, liquid starch sugar, vegetable oil and other ingredients together, make the material dissolves.
2. When the temperature of material liquid rise to 70 ¡æ, shear with high-speed and emulsify 5-15 minutes.
3.After fully homogeneous under high pressure with homogenizer to spray drying tower and dry. The homogeneous pressure is for 20-35 MPa.
4. Spray drying, adjust import and export wind temperature, spray pressure and nozzle according to the actual production situation. Wind in 160-180 ¡æ, wind out 80-100 ¡æ, wind pressure 10-20 MPa.
5.The powder packaging ,after cooling below 35 ¡æwith the fluidized bed, add anticaking agent, stirring for 10 minutes ,then packaging.